Published May 13, 2011 | Journal article | Version v1 | https://doi.org/10.1111/j.1600-0722.2011.00829.x

Fracture stability of anterior zirconia crowns with different core designs and veneered using the layering or the press-over technique

Additional details

Dates

Issued
May 13, 2011

References

  1. ÅKESSON, J., SUNDH, A., & SJÖGREN, G. (2009). Fracture resistance of all‐ceramic crowns placed on a preparation with a slice‐formed finishing line. Journal of Oral Rehabilitation, 36(7), 516–523. https://doi.org/10.1111/j.1365-2842.2009.01962.x
  2. Beuer, F., Schweiger, J., Eichberger, M., Kappert, H. F., Gernet, W., & Edelhoff, D. (2009). High-strength CAD/CAM-fabricated veneering material sintered to zirconia copings — A new fabrication mode for all-ceramic restorations. Dental Materials, 25(1), 121–128. https://doi.org/10.1016/j.dental.2008.04.019
  3. Kohorst, P., Herzog, T. J., Borchers, L., & Stiesch‐Scholz, M. (2007). Load‐bearing capacity of all‐ceramic posterior four‐unit fixed partial dentures with different zirconia frameworks. European Journal of Oral Sciences, 115(2), 161–166. https://doi.org/10.1111/j.1600-0722.2007.00429.x
  4. Limkangwalmongkol, P., Chiche, G. J., & Blatz, M. B. (2007). Precision of Fit of Two Margin Designs for Metal‐Ceramic Crowns. Journal of Prosthodontics, 16(4), 233–237. https://doi.org/10.1111/j.1532-849x.2007.00186.x
  5. Holden, J. E., Goldstein, G. R., Hittelman, E. L., & Clark, E. A. (2009). Comparison of the Marginal Fit of Pressable Ceramic to Metal Ceramic Restorations. Journal of Prosthodontics, 18(8), 645–648. https://doi.org/10.1111/j.1532-849x.2009.00497.x
  6. Potiket, N., Chiche, G., & Finger, I. M. (2004). In vitro fracture strength of teeth restored with different all-ceramic crown systems. The Journal of Prosthetic Dentistry, 92(5), 491–495. https://doi.org/10.1016/j.prosdent.2004.09.001
  7. KOHORST, P., BRINKMANN, H., DITTMER, M. P., BORCHERS, L., & STIESCH, M. (2010). Influence of the veneering process on the marginal fit of zirconia fixed dental prostheses. Journal of Oral Rehabilitation, 37(4), 283–291. https://doi.org/10.1111/j.1365-2842.2009.02053.x
  8. Faul, F., Erdfelder, E., Lang, A.-G., & Buchner, A. (2007). G*Power 3: A flexible statistical power analysis program for the social, behavioral, and biomedical sciences. Behavior Research Methods, 39(2), 175–191. https://doi.org/10.3758/bf03193146
  9. Reich, S., Petschelt, A., & Lohbauer, U. (2008). The effect of finish line preparation and layer thickness on the failure load and fractography of ZrO2 copings. The Journal of Prosthetic Dentistry, 99(5), 369–376. https://doi.org/10.1016/s0022-3913(08)60085-2
  10. Michalakis, K. X., Stratos, A., Hirayama, H., Kang, K., Touloumi, F., & Oishi, Y. (2009). Fracture Resistance of Metal Ceramic Restorations with Two Different Margin Designs After Exposure to Masticatory Simulation. The Journal of Prosthetic Dentistry, 102(3), 172–178. https://doi.org/10.1016/s0022-3913(09)60141-4
  11. Finite element analysis studies of an all-ceramic crown on a first premolar
  12. Van Dalen, A., Feilzer, A. J., & Kleverlaan, C. J. (2008). In Vitro Exploration and Finite Element Analysis of Failure Mechanisms of Resin‐Bonded Fixed Partial Dentures. Journal of Prosthodontics, 17(7), 555–561. https://doi.org/10.1111/j.1532-849x.2008.00349.x
  13. Anusavice, K. J., Hojjatie, B., & Dehoff, P. H. (1986). Influence of Metal Thickness on Stress Distribution in Metal-Ceramic Crowns. Journal of Dental Research, 65(9), 1173–1178. https://doi.org/10.1177/00220345860650091201
  14. The fracture resistance of all-ceramic crowns on supporting structures with different elastic moduli
  15. In vitro fracture force and marginal adaptation of ceramic crowns fixed on natural and artificial teeth
  16. Kiliaridis, S., Kjellberg, H., Wenneberg, B., & Engström, C. (1993). The relationship between maximal bite force, bite force endurance, and facial morphology during growth: A cross-sectional study. Acta Odontologica Scandinavica, 51(5), 323–331. https://doi.org/10.3109/00016359309040583

Citations

  1. https://doi.org/10.5005/jp-journals-10024-3837
  2. Côcco, L. C., Nuernberg, G. G. V., & Cunico, M. W. M. (2024). Characterization of dental prosthesis based on nano-fluorapatite glass-ceramic fabricated by shell sintering technology. Journal of Manufacturing Processes, 109, 501–511. https://doi.org/10.1016/j.jmapro.2023.12.047
  3. https://doi.org/10.5005/jp-journals-10019-1358
  4. Shelar, P., Abdolvand, H., & Butler, S. (2021). On the behaviour of zirconia-based dental materials: A review. Journal of the Mechanical Behavior of Biomedical Materials, 124, 104861. https://doi.org/10.1016/j.jmbbm.2021.104861
  5. https://doi.org/10.3390/app11052129
  6. Marchionatti, A. M. E., Aurélio, I. L., & May, L. G. (2018). Does veneering technique affect the flexural strength or load-to-failure of bilayer Y-TZP? A systematic review and meta-analysis. The Journal of Prosthetic Dentistry, 119(6), 916–924. https://doi.org/10.1016/j.prosdent.2017.11.013
  7. Obermeier, M., Ristow, O., Erdelt, K., & Beuer, F. (2017). Mechanical performance of cement– and screw–retained all–ceramic single crowns on dental implants. Clinical Oral Investigations, 22(2), 981–991. https://doi.org/10.1007/s00784-017-2178-z
  8. Rand, A., Kohorst, P., Greuling, A., Borchers, L., & Stiesch, M. (2016). Stress Distribution in All-Ceramic Posterior 4-Unit Fixed Dental Prostheses Supported in Different Ways. Implant Dentistry, 25(4), 485–491. https://doi.org/10.1097/id.0000000000000429
  9. https://doi.org/10.1111/jopr.12489
  10. https://doi.org/10.1111/jopr.12490
  11. https://doi.org/10.17567/ataunidfd.290299
  12. https://doi.org/10.4047/jap.2015.7.6.454
  13. Schmitter, M., Schweiger, M., Mueller, D., & Rues, S. (2014). Effect on in vitro fracture resistance of the technique used to attach lithium disilicate ceramic veneer to zirconia frameworks. Dental Materials, 30(2), 122–130. https://doi.org/10.1016/j.dental.2013.10.008
  14. https://doi.org/10.1111/jopr.12130
  15. https://doi.org/10.1111/jopr.12236
  16. Miyazaki, T., Nakamura, T., Matsumura, H., Ban, S., & Kobayashi, T. (2013). Current status of zirconia restoration. Journal of Prosthodontic Research, 57(4), 236–261. https://doi.org/10.1016/j.jpor.2013.09.001
  17. https://doi.org/10.4012/dmj.2013-039
  18. https://doi.org/10.3109/00016357.2012.741706
  19. https://doi.org/10.4028/www.scientific.net/kem.512-515.1779