Influence of Preliminary Damage on the Load‐Bearing Capacity of Zirconia Fixed Dental Prostheses
Description
AbstractPurpose:The objective of this investigation was to evaluate the influence of differently shaped preliminary cuts in combination with artificial aging on the load‐bearing capacity of four‐unit zirconia fixed dental prostheses (FDPs).Materials and Methods:Forty frameworks were fabricated from white‐stage zirconia blanks (InCeram YZ, Vita) by means of a computer‐aided design/computer‐aided manufacturing system (Cerec inLab, Sirona). Frameworks were divided into four homogeneous groups with ten specimens each. Prior to veneering, frameworks of two groups were "damaged" by defined saw cuts of different dimensions, to simulate accidental flaws generated during shape cutting. After the veneering process, FDPs, with the exception of a control group without preliminary damage, were subjected to thermal and mechanical cycling (TMC) during 200 days storage in distilled water at 36°C. Following the aging procedure, all specimens were loaded until fracture, and forces at fracture were recorded. The statistical analysis of force at fracture data was performed using two‐way ANOVA, with the level of significance chosen at 0.05.Results:Neither type of preliminary mechanical damage significantly affected the load‐bearing capacity of FDPs. In contrast, artificial aging by TMC proved to have a significant influence on the load‐bearing capacity of both the undamaged and the predamaged zirconia restorations (p< 0.001); however, even though load‐bearing capacity decreased by about 20% due to simulated aging, the FDPs still showed mean load‐bearing capacities of about 1600 N.Conclusions:The results of this study reveal that zirconia restorations have a high tolerance regarding mechanical damages. Irrespective of these findings, damage to zirconia ceramics during production or finishing should be avoided, as this may nevertheless lead to subcritical crack growth and, eventually, catastrophic failure. Furthermore, to ensure long‐term clinical success, the design of zirconia restorations has to accommodate the decrease in load‐bearing capacity due to TMC in the oral environment.
Additional details
Identifiers
Dates
- Issued
-
August 16, 2010
References
- Kohorst, P., Herzog, T. J., Borchers, L., & Stiesch‐Scholz, M. (2007). Load‐bearing capacity of all‐ceramic posterior four‐unit fixed partial dentures with different zirconia frameworks. European Journal of Oral Sciences, 115(2), 161–166. https://doi.org/10.1111/j.1600-0722.2007.00429.x
- Kohorst, P., Dittmer, M. P., Borchers, L., & Stiesch-Scholz, M. (2008). Influence of cyclic fatigue in water on the load-bearing capacity of dental bridges made of zirconia. Acta Biomaterialia, 4(5), 1440–1447. https://doi.org/10.1016/j.actbio.2008.04.012
- Hannink, R. H. J., Kelly, P. M., & Muddle, B. C. (2000). Transformation Toughening in Zirconia‐Containing Ceramics. Journal of the American Ceramic Society, 83(3), 461–487. https://doi.org/10.1111/j.1151-2916.2000.tb01221.x
- Aboushelib, M. N., de Jager, N., Kleverlaan, C. J., & Feilzer, A. J. (2007). Effect of loading method on the fracture mechanics of two layered all-ceramic restorative systems. Dental Materials, 23(8), 952–959. https://doi.org/10.1016/j.dental.2006.06.036
- Kun Lee, S., Tandon, R., Readey, M. J., & Lawn, B. R. (2000). Scratch Damage in Zirconia Ceramics. Journal of the American Ceramic Society, 83(6), 1428–1432. https://doi.org/10.1111/j.1151-2916.2000.tb01406.x
- Zhang, Y., & Lawn, B. (2004). Long‐term strength of ceramics for biomedical applications. Journal of Biomedical Materials Research Part B: Applied Biomaterials, 69B(2), 166–172. https://doi.org/10.1002/jbm.b.20039
- Luthardt, R. G., Holzhüter, M., Sandkuhl, O., Herold, V., Schnapp, J. D., Kuhlisch, E., & Walter, M. (2002). Reliability and Properties of Ground Y-TZP-Zirconia Ceramics. Journal of Dental Research, 81(7), 487–491. https://doi.org/10.1177/154405910208100711
- Luthardt, R. G., Holzhüter, M. S., Rudolph, H., Herold, V., & Walter, M. H. (2004). CAD/CAM-machining effects on Y-TZP zirconia. Dental Materials, 20(7), 655–662. https://doi.org/10.1016/j.dental.2003.08.007
- Dittmer, M. P., Kohorst, P., Borchers, L., & Stiesch-Scholz, M. (2009). Finite element analysis of a four-unit all-ceramic fixed partial denture. Acta Biomaterialia, 5(4), 1349–1355. https://doi.org/10.1016/j.actbio.2008.11.015
- Wiederhorn, S. M. (1968). Moisture assisted crack growth in ceramics. International Journal of Fracture Mechanics, 4(2), 171–177. https://doi.org/10.1007/bf00188945
- Chevalier, J., Olagnon, C., & Fantozzi, G. (1999). Subcritical Crack Propagation in 3Y‐TZP Ceramics: Static and Cyclic Fatigue. Journal of the American Ceramic Society, 82(11), 3129–3138. https://doi.org/10.1111/j.1151-2916.1999.tb02213.x
- Guo, X. (2004). Property Degradation of Tetragonal Zirconia Induced by Low-Temperature Defect Reaction with Water Molecules. Chemistry of Materials, 16(21), 3988–3994. https://doi.org/10.1021/cm040167h
- Chevalier, J., Cales, B., & Drouin, J. M. (1999). Low‐Temperature Aging of Y‐TZP Ceramics. Journal of the American Ceramic Society, 82(8), 2150–2154. https://doi.org/10.1111/j.1151-2916.1999.tb02055.x
- Garvie, R. C., Urbani, C., Kennedy, D. R., & McNeuer, J. C. (1984). Biocompatibility of magnesia-partially stabilized zirconia (Mg-PSZ) ceramics. Journal of Materials Science, 19(10), 3224–3228. https://doi.org/10.1007/bf00549808
- Thompson, I., & Rawlings, R. D. (1990). Mechanical behaviour of zirconia and zirconia-toughened alumina in a simulated body environment. Biomaterials, 11(7), 505–508. https://doi.org/10.1016/0142-9612(90)90066-y
- Rosentritt, M., Behr, M., Gebhard, R., & Handel, G. (2006). Influence of stress simulation parameters on the fracture strength of all-ceramic fixed-partial dentures. Dental Materials, 22(2), 176–182. https://doi.org/10.1016/j.dental.2005.04.024
- Ritter, J. E., Vicedomine, M., Breder, K., & Jakus, K. (1985). Dynamic fatigue of indented, soda-lime glass as a function of temperature. Journal of Materials Science, 20(8), 2868–2872. https://doi.org/10.1007/bf00553050
- Addison, O., Fleming, G. J. P., & Marquis, P. M. (2003). The effect of thermocycling on the strength of porcelain laminate veneer (PLV) materials. Dental Materials, 19(4), 291–297. https://doi.org/10.1016/s0109-5641(02)00046-5
- The fracture resistance of all‐ceramic crowns on supporting structures with different elastic moduli
- Stiesch-Scholz, M., Schulz, K., & Borchers, L. (2006). In vitro fracture resistance of four-unit fiber-reinforced composite fixed partial dentures. Dental Materials, 22(4), 374–381. https://doi.org/10.1016/j.dental.2005.04.040
- Parfitt, G. J. (1960). Measurement of the Physiological Mobility of Individual Teeth in an Axial Direction. Journal of Dental Research, 39(3), 608–618. https://doi.org/10.1177/00220345600390032201
- Elektronische Untersuchung zur Reproduzierbarkeit des okklusalen Traumas [Electronic studies on the reproducibility of occlusal trauma]
- VON STEYERN, P. V., CARLSON, P., & NILNER, K. (2005). All‐ceramic fixed partial dentures designed according to the DC‐Zirkon® technique. A 2‐year clinical study. Journal of Oral Rehabilitation, 32(3), 180–187. https://doi.org/10.1111/j.1365-2842.2004.01437.x
- Marx, R., Jungwirth, F., & Walter, P.-O. (2004). Threshold intensity factors as lower boundaries for crack propagation in ceramics. BioMedical Engineering OnLine, 3(1). https://doi.org/10.1186/1475-925x-3-41
- Deng, Y., Lawn, B. R., & Lloyd, I. K. (2002). Characterization of damage modes in dental ceramic bilayer structures. Journal of Biomedical Materials Research, 63(2), 137–145. https://doi.org/10.1002/jbm.10091
1–25 of 45
Citations
- Zimmermann, M., Ender, A., & Mehl, A. (2020). Influence of CAD/CAM Fabrication and Sintering Procedures on the Fracture Load of Full-Contour Monolithic Zirconia Crowns as a Function of Material Thickness. Operative Dentistry, 45(2), 219–226. https://doi.org/10.2341/19-086-l
- Wang, W., Yu, H., Liu, Y., Jiang, X., & Gao, B. (2019). Trueness analysis of zirconia crowns fabricated with 3-dimensional printing. The Journal of Prosthetic Dentistry, 121(2), 285–291. https://doi.org/10.1016/j.prosdent.2018.04.012
- Mühlemann, S., Benic, G. I., Fehmer, V., Hämmerle, C. H. F., & Sailer, I. (2019). Randomized controlled clinical trial of digital and conventional workflows for the fabrication of zirconia-ceramic posterior fixed partial dentures. Part II: Time efficiency of CAD-CAM versus conventional laboratory procedures. The Journal of Prosthetic Dentistry, 121(2), 252–257. https://doi.org/10.1016/j.prosdent.2018.04.020
- Zarkovic Gjurin, S., Özcan, M., & Oblak, C. (2018). Zirconia ceramic fixed partial dentures after cyclic fatigue tests and clinical evaluation: a systematic review. Advances in Applied Ceramics, 118(1-2), 62–69. https://doi.org/10.1080/17436753.2018.1507428
- Amaral, M., Villefort, R. F., Melo, R. M., Pereira, G. K. R., Zhang, Y., Valandro, L. F., & Bottino, M. A. (2017). Fatigue limit of monolithic Y-TZP three-unit-fixed dental prostheses: Effect of grinding at the gingival zone of the connector. Journal of the Mechanical Behavior of Biomedical Materials, 72, 159–162. https://doi.org/10.1016/j.jmbbm.2017.03.002
- Kirsch, C., Ender, A., Attin, T., & Mehl, A. (2016). Trueness of four different milling procedures used in dental CAD/CAM systems. Clinical Oral Investigations, 21(2), 551–558. https://doi.org/10.1007/s00784-016-1916-y
- Antioquia, U. de ., Suárez B, N. T., Escobar Restrepo, J. C., Antioquia, U. de ., Latorre Correa, F., Antioquia, U. de ., Villarraga Ossa, J., & Antioquia, U. de . (2015). Comportamiento estático de un pilar de circona sometido envejecimiento artificial. Método de elementos finitos. Revista Facultad De Odontología, 27(1). https://doi.org/10.17533/udea.rfo.v27n1a2
- Preis, V., Behr, M., Hahnel, S., Handel, G., & Rosentritt, M. (2012). In vitro failure and fracture resistance of veneered and full-contour zirconia restorations. Journal of Dentistry, 40(11), 921–928. https://doi.org/10.1016/j.jdent.2012.07.010
- Sarafidou, K., Stiesch, M., Dittmer, M. P., Jörn, D., Borchers, L., & Kohorst, P. (2011). Load-bearing capacity of artificially aged zirconia fixed dental prostheses with heterogeneous abutment supports. Clinical Oral Investigations, 16(3), 961–968. https://doi.org/10.1007/s00784-011-0569-0