Published April 2012 | Journal article | Version v1 | https://doi.org/10.1016/j.jpor.2011.09.002

Effect of thermal expansion mismatch on the Y-TZP/veneer interfacial adhesion determined by strain energy release rate

Additional details

Dates

Issued
April 2012

References

  1. Denry, I., & Kelly, J. R. (2008). State of the art of zirconia for dental applications. Dental Materials, 24(3), 299–307. https://doi.org/10.1016/j.dental.2007.05.007
  2. Manicone, P. F., Rossi Iommetti, P., & Raffaelli, L. (2007). An overview of zirconia ceramics: Basic properties and clinical applications. Journal of Dentistry, 35(11), 819–826. https://doi.org/10.1016/j.jdent.2007.07.008
  3. Conrad, H. J., Seong, W.-J., & Pesun, I. J. (2007). Current ceramic materials and systems with clinical recommendations: A systematic review. The Journal of Prosthetic Dentistry, 98(5), 389–404. https://doi.org/10.1016/s0022-3913(07)60124-3
  4. VON STEYERN, P. V., CARLSON, P., & NILNER, K. (2005). All‐ceramic fixed partial dentures designed according to the DC‐Zirkon® technique. A 2‐year clinical study. Journal of Oral Rehabilitation, 32(3), 180–187. https://doi.org/10.1111/j.1365-2842.2004.01437.x
  5. Sailer, I., Pjetursson, B. E., Zwahlen, M., & Hämmerle, C. H. F. (2007). A systematic review of the survival and complication rates of all‐ceramic and metal–ceramic reconstructions after an observation period of at least 3 years. Part II: fixed dental prostheses. Clinical Oral Implants Research, 18(s3), 86–96. https://doi.org/10.1111/j.1600-0501.2007.01468.x
  6. Complications with Cercon restorations in the first five years in situ
  7. Fischer, J., Stawarczyk, B., & Hämmerle, C. H. F. (2008). Flexural strength of veneering ceramics for zirconia. Journal of Dentistry, 36(5), 316–321. https://doi.org/10.1016/j.jdent.2008.01.017
  8. Fischer, J., Stawarczyk, B., Trottmann, A., & Hämmerle, C. H. F. (2009). Impact of thermal properties of veneering ceramics on the fracture load of layered Ce-TZP/A nanocomposite frameworks. Dental Materials, 25(3), 326–330. https://doi.org/10.1016/j.dental.2008.08.001
  9. DeHoff, P. H., Barrett, A. A., Lee, R. B., & Anusavice, K. J. (2008). Thermal compatibility of dental ceramic systems using cylindrical and spherical geometries. Dental Materials, 24(6), 744–752. https://doi.org/10.1016/j.dental.2007.08.008
  10. Fischer, J., Stawarzcyk, B., Trottmann, A., & Hämmerle, C. H. F. (2009). Impact of thermal misfit on shear strength of veneering ceramic/zirconia composites. Dental Materials, 25(4), 419–423. https://doi.org/10.1016/j.dental.2008.09.003
  11. Lenz, J., & Kessel, S. (1998). Thermal stresses in metal–ceramic specimens for the ISO crack initiation test (three-point flexure bond test). Dental Materials, 14(4), 277–280. https://doi.org/10.1016/s0109-5641(98)00039-6
  12. Bagby, M., Marshall, S. J., & Marshall, G. W. (1990). Metal ceramic compatibility: A review of the literature. The Journal of Prosthetic Dentistry, 63(1), 21–25. https://doi.org/10.1016/0022-3913(90)90259-f
  13. Aboushelib, M. N., Feilzer, A. J., de Jager, N., & Kleverlaan, C. J. (2008). Prestresses in bilayered all‐ceramic restorations. Journal of Biomedical Materials Research Part B: Applied Biomaterials, 87B(1), 139–145. https://doi.org/10.1002/jbm.b.31083
  14. Aboushelib, M. N., Kleverlaan, C. J., & Feilzer, A. J. (2006). Microtensile bond strength of different components of core veneered all-ceramic restorations. Dental Materials, 22(9), 857–863. https://doi.org/10.1016/j.dental.2005.11.014
  15. FISCHER, J., STAWARCZYK, B., TOMIC, M., STRUB, J. R., & HÄMMERLE, C. H. F. (2007). Effect of Thermal Misfit between Different Veneering Ceramics and Zirconia Frameworks on in vitro Fracture Load of Single Crowns. Dental Materials Journal, 26(6), 766–772. https://doi.org/10.4012/dmj.26.766
  16. Dündar, M., Özcan, M., Gökçe, B., Çömlekoğlu, E., Leite, F., & Valandro, L. F. (2007). Comparison of two bond strength testing methodologies for bilayered all-ceramics. Dental Materials, 23(5), 630–636. https://doi.org/10.1016/j.dental.2006.05.004
  17. Al-Dohan, H. M., Yaman, P., Dennison, J. B., Razzoog, M. E., & Lang, B. R. (2004). Shear strength of core-veneer interface in bi-layered ceramics. The Journal of Prosthetic Dentistry, 91(4), 349–355. https://doi.org/10.1016/j.prosdent.2004.02.009
  18. Charalambides, P. G., Lund, J., Evans, A. G., & McMeeking, R. M. (1989). A Test Specimen for Determining the Fracture Resistance of Bimaterial Interfaces. Journal of Applied Mechanics, 56(1), 77–82. https://doi.org/10.1115/1.3176069
  19. New approach for evaluating metal-porcelain interfacial bonding
  20. Tholey, M. J., Waddell, J. N., & Swain, M. V. (2007). Influence of the bonder on the adhesion of porcelain to machined titanium as determined by the strain energy release rate. Dental Materials, 23(7), 822–828. https://doi.org/10.1016/j.dental.2006.06.022
  21. Homann, F., Waddell, J. N., & Swain, M. V. (2006). Influence of water, loading rate and bonder on the adhesion of porcelain to titanium. Journal of Dentistry, 34(7), 485–490. https://doi.org/10.1016/j.jdent.2005.11.004
  22. Göstemeyer, G., Jendras, M., Dittmer, M. P., Bach, F.-W., Stiesch, M., & Kohorst, P. (2010). Influence of cooling rate on zirconia/veneer interfacial adhesion. Acta Biomaterialia, 6(12), 4532–4538. https://doi.org/10.1016/j.actbio.2010.06.026
  23. Bonding mechanisms in layered systems for dental use
  24. Swain, M. V. (2009). Unstable cracking (chipping) of veneering porcelain on all-ceramic dental crowns and fixed partial dentures. Acta Biomaterialia, 5(5), 1668–1677. https://doi.org/10.1016/j.actbio.2008.12.016
  25. Timoshenko, S. (1925). Analysis of Bi-Metal Thermostats. Journal of the Optical Society of America, 11(3), 233. https://doi.org/10.1364/josa.11.000233

1–25 of 32

Citations

  1. Awan, T. I., Afsheen, S., & Kausar, S. (2025). Emerging Trends and Issues Related to Thin Films. In Thin Film Deposition Techniques (pp. 241–278). Springer Nature Singapore. https://doi.org/10.1007/978-981-96-1364-9_9
  2. Zhao, W., Sun, J., Ding, H., Manzoor, S., Yu, H., Bai, J., & Tsoi, J. K. H. (2025). High-strength DLP-printed zirconia for ultra-thin dental veneers. Dental Materials, 41(11), 1430–1441. https://doi.org/10.1016/j.dental.2025.08.005
  3. Vohra, M., Ahmed, N., Keskar, V., & Shenoy, A. (2024). A Comparison of the Edge Testing of Indirect Composite Layered Zirconia Crowns and Monolithic Zirconia Crowns Without Aging: An In Vitro Study. Cureus. https://doi.org/10.7759/cureus.62080
  4. Worpenberg, C., Stiesch, M., Eisenburger, M., Breidenstein, B., Busemann, S., & Greuling, A. (2023). The effect of surface treatments on the adhesive bond in all-ceramic dental crowns using four-point bending and dynamic loading tests. Journal of the Mechanical Behavior of Biomedical Materials, 139, Article 105686. https://doi.org/10.1016/j.jmbbm.2023.105686
  5. https://doi.org/10.1590/1678-7757-2022-0421
  6. Şahin, C. (2022). Double veneering, low-temperature porcelain, and total glaze application methods to overcome failures of zirconia-based restorations. Clinical Oral Investigations, 26(5), 4081–4089. https://doi.org/10.1007/s00784-022-04376-2
  7. Li, Q.-L., Jiang, Y.-Y., Wei, Y.-R., Swain, M. V., Yao, M.-F., Li, D.-S., Wei, T., Jian, Y.-T., Zhao, K., & Wang, X.-D. (2022). The influence of yttria content on the microstructure, phase stability and mechanical properties of dental zirconia. Ceramics International, 48(4), 5361–5368. https://doi.org/10.1016/j.ceramint.2021.11.079
  8. Hensel, J., Reise, M., Liebermann, A., Buser, R., & Stawarczyk, B. (2022). Impact of multiple firings on thermal properties and bond strength of veneered zirconia restorations. Journal of the Mechanical Behavior of Biomedical Materials, 128, 105134. https://doi.org/10.1016/j.jmbbm.2022.105134
  9. Talibi, M., Kaur, K., & Parmar, H. (2022). Do you know your ceramics? Part 5: zirconia. British Dental Journal, 232(5), 311–316. https://doi.org/10.1038/s41415-022-3997-0
  10. https://doi.org/10.34172/jlms.2022.31
  11. Shelar, P., Abdolvand, H., & Butler, S. (2021). On the behaviour of zirconia-based dental materials: A review. Journal of the Mechanical Behavior of Biomedical Materials, 124, 104861. https://doi.org/10.1016/j.jmbbm.2021.104861
  12. Lu, Y., Mei, Z., Lou, Y., Yue, L., Chen, X., Sun, J., Wan, Z., & Yu, H. (2020). Schwickerath adhesion tests of porcelain veneer and stereolithographic additive-manufactured zirconia. Ceramics International, 46(10), 16572–16577. https://doi.org/10.1016/j.ceramint.2020.03.228
  13. https://doi.org/10.2341/19-023-l
  14. Sawada, T., Wagner, V., Schille, C., Spintzyk, S., Schweizer, E., & Geis-Gerstorfer, J. (2019). Effect of slow-cooling protocol on biaxial flexural strengths of bilayered porcelain-ceria-stabilized zirconia/alumina nanocomposite (Ce-TZP/A) disks. Dental Materials, 35(2), 270–282. https://doi.org/10.1016/j.dental.2018.11.024
  15. Yamauchi, S., Miura, S., Kasahara, S., Sun, J., & Egusa, H. (2019). A thick frame decreases the fracture toughness of veneering ceramics used for zirconia-based all-ceramic restorations. Journal of Prosthodontic Research, 63(2), 184–192. https://doi.org/10.1016/j.jpor.2018.11.007
  16. Swain, M. V., Gee, C., & Li, K. C. (2018). Influence of ageing on glass and resin bonding of dental glass-ceramic veneer adhesion to zirconia: A fracture mechanics analysis and interpretation. Acta Biomaterialia, 74, 454–463. https://doi.org/10.1016/j.actbio.2018.04.049
  17. Sawada, T., Schille, C., Wagner, V., Spintzyk, S., Schweizer, E., & Geis-Gerstorfer, J. (2018). Biaxial flexural strength of the bilayered disk composed of ceria-stabilized zirconia/alumina nanocomposite (Ce-TZP/A) and veneering porcelain. Dental Materials, 34(8), 1199–1210. https://doi.org/10.1016/j.dental.2018.05.003
  18. van Vuuren, W.-A. J., Wong, P., Al-Amleh, B., Lyons, K. M., Li, K. C., & Waddell, J. N. (2018). Effect of a glaze layer on adhesion energy between resin cements to zirconia ceramic. International Journal of Adhesion and Adhesives, 84, 451–456. https://doi.org/10.1016/j.ijadhadh.2018.03.003
  19. Ramos, V., & Øilo, M. (2018). Thermal cracks of implant-based zirconia four-unit restorations: A fractographic analysis of two restorations fractured during production. The Journal of Prosthetic Dentistry, 120(3), 327–330. https://doi.org/10.1016/j.prosdent.2017.11.018
  20. https://doi.org/10.3390/ma11010077
  21. Gee, C., Weddell, J. N., & Swain, M. V. (2017). Comparison of three and four point bending evaluation of two adhesive bonding systems for glass-ceramic zirconia bi-layered ceramics. Dental Materials, 33(9), 1004–1011. https://doi.org/10.1016/j.dental.2017.06.007
  22. Jansen van Vuuren, W.-A., Jansen van Vuuren, L., Torr, B., & Waddell, J. N. (2016). Adhesion between zirconia and indirect composite resin. International Journal of Adhesion and Adhesives, 69, 72–78. https://doi.org/10.1016/j.ijadhadh.2016.03.011
  23. Mirsayar, M. M., & Park, P. (2016). Modified maximum tangential stress criterion for fracture behavior of zirconia/veneer interfaces. Journal of the Mechanical Behavior of Biomedical Materials, 59, 236–240. https://doi.org/10.1016/j.jmbbm.2015.11.037
  24. Alghazzawi, T. F., & Janowski, G. M. (2016). Effect of liner and porcelain application on zirconia surface structure and composition. International Journal of Oral Science, 8(3), 164–171. https://doi.org/10.1038/ijos.2016.20
  25. https://doi.org/10.1111/ffe.12394

1–25 of 37