Published December 7, 2007 | Journal article | Version v1 | https://doi.org/10.1002/jbm.a.31713

Evaluation of the skin sensitizing potential of biodegradable magnesium alloys

Description

AbstractCorroding metals made of magnesium alloys represent a new class of degradable implants for musculoskeletal surgery. These implants may be associated with skin sensitizing reactions because of the release of metal ions. This study was conducted to compare the sensitizing potential of four different magnesium alloys (AZ31, AZ91, WE43, and LAE442) to current implant materials such as titanium (TiAl6V4) and a degradable polymer (SR‐PLA96). Solutions and solid chips of these materials were prepared and tested in 156 guinea pigs according to the Magnusson–Kligman test. A standard allergen (hydroxy‐cinnamon‐aldehyde) causing allergic erythema was used as positive control and a standard irritant (sodium‐lauryl‐sulfate) causing local skin irritation for less than 24 h was used as negative control. All erythema were graded immediately and 24 h after patch removal by three independent observers. Histomorphological analyses were performed on skin biopsies taken 24 h after patch removal. We found that initial erythema in animals treated with solid chips diminished within 24 h and were caused by local skin irritation. Local skin irritation was also determined in erythema remaining for 24 h after patch removal in animals treated with dissolved test materials. No allergenic reactions according to the histomorphological criteria were observed in skin biopsies. We conclude that no skin sensitizing potential were detected for standard materials as well as for all tested magnesium alloys by the used methods. © 2007 Wiley Periodicals, Inc. J Biomed Mater Res, 2008

Additional details

Dates

Issued
December 7, 2007

References

  1. Weiler, A., Hoffmann, R. F. G., Stähelin, A. C., Helling, H., & Südkamp, N. P. (2000). Biodegradable Implants in Sports Medicine: The Biological Base. Arthroscopy, 16(3), 305–321. https://doi.org/10.1016/s0749-8063(00)90055-0
  2. Claes, L. E. (1992). Mechanical characterization of biodegradable implants. Clinical Materials, 10(1-2), 41–46. https://doi.org/10.1016/0267-6605(92)90083-6
  3. Wintermantel, E., & Ha, S.-W. (1996). Biokompatible Werkstoffe und Bauweisen. Springer Berlin Heidelberg. https://doi.org/10.1007/978-3-662-06077-3
  4. Witte, F., Kaese, V., Haferkamp, H., Switzer, E., Meyer-Lindenberg, A., Wirth, C. J., & Windhagen, H. (2005). In vivo corrosion of four magnesium alloys and the associated bone response. Biomaterials, 26(17), 3557–3563. https://doi.org/10.1016/j.biomaterials.2004.09.049
  5. McBRIDE, E. D. (1938). ABSORBABLE METAL IN BONE SURGERY: A FURTHER REPORT ON THE USE OF MAGNESIUM ALLOYS. Journal of the American Medical Association, 111(27), 2464. https://doi.org/10.1001/jama.1938.02790530018007
  6. Hallab, N., Merritt, K., & Jacobs, J. J. (2001). Metal Sensitivity in Patients with Orthopaedic Implants. The Journal of Bone and Joint Surgery-American Volume, 83(3), 428–436. https://doi.org/10.2106/00004623-200103000-00017
  7. Merritt, K., & Rodrigo, J. J. (1996). Immune Response to Synthetic Materials: Sensitization of Patients Receiving Orthopaedic Implants. Clinical Orthopaedics and Related Research, 326, 71–79. https://doi.org/10.1097/00003086-199605000-00009
  8. Magnusson, B., & Kligman, A. M. (1969). The Identification of Contact Allergens by Animal Assay. the Guinea Pig Maximization Test**From the Department of Dermatology, University of Gothenburg, Sahlgrenska Sjukhuset, Gothenburg, Sweden and the Department of Dermatology, University of Pennsylvania School of Medicine, Philadelphia, Pennsylvania 19104. Journal of Investigative Dermatology, 52(3), 268–276. https://doi.org/10.1038/jid.1969.42
  9. Kligman, A. M., & Basketter, D. A. (1995). A critical commentary and updating of the guinea pig maximization test. Contact Dermatitis, 32(3), 129–134. https://doi.org/10.1111/j.1600-0536.1995.tb00801.x
  10. Hunziker, N., & Olmos, L. (1976). A propos des basophiles dans l’infiltrat de l’eczéma experimental chez le cobaye. Dermatology, 152(5), 270–280. https://doi.org/10.1159/000251252
  11. Lindberg, L. R., Johnell, O., & Linder, L. (1988). Reactions in rat gluteal muscle to titanium implants. Biomaterials, 9(6), 546. https://doi.org/10.1016/0142-9612(88)90053-1
  12. Turk, J. L., & Parker, D. (1977). Sensitization With Cr, Ni, and Zr Salts and Allergic Type Granuloma Formation in The Guinea Pig. Journal of Investigative Dermatology, 68(6), 341–345. https://doi.org/10.1111/1523-1747.ep12496465
  13. Zissu, D., Binet, S., & Cavelier, C. (1996). Patch testing with beryllium alloy samples in guinea pigs. Contact Dermatitis, 34(3), 196–200. https://doi.org/10.1111/j.1600-0536.1996.tb02173.x
  14. Robinson, M. K., Fletcher, E. R., Johnson, G. R., Wyder, W. E., & Maurer, J. K. (1990). Value of the Cutaneous Basophil Hypersensitivity (CBH) Response for Distinguishing Weak Contact Sensitization from Irritation Reactions in the Guinea Pig. Journal of Investigative Dermatology, 94(5), 636–643. https://doi.org/10.1111/1523-1747.ep12876210
  15. The effect of selected immunomodulating agents on experimental contact reactions
  16. Groth, O., & Skoog, M. (1979). Measurement and differentiation of the cellular infiltrate in expermiental allergic contact dermatitis. Acta Dermato-Venereologica, 59(2), 129–134. https://doi.org/10.2340/0001555559129134
  17. Sjögren, F., & Anderson, C. (2000). The spectrum of inflammatory cell response to dimethyl sulfoxide. Contact Dermatitis, 42(4), 216–221. https://doi.org/10.1034/j.1600-0536.2000.042004216.x
  18. Witte, F., Fischer, J., Nellesen, J., Crostack, H.-A., Kaese, V., Pisch, A., Beckmann, F., & Windhagen, H. (2006). In vitro and in vivo corrosion measurements of magnesium alloys. Biomaterials, 27(7), 1013–1018. https://doi.org/10.1016/j.biomaterials.2005.07.037
  19. Thomas, P., Summer, B., Sander, C. A., Przybilla, B., Thomas, M., & Naumann, T. (2000). Intolerance of osteosynthesis material: evidence of dichromate contact allergy with concomitant oligoclonal T‐cell infiltrate and TH1‐type cytokine expression in the peri‐implantar tissue. Allergy, 55(10), 969–972. https://doi.org/10.1034/j.1398-9995.2000.00619.x
  20. Hierholzer, S., Hierholzer, G., Sauer, K. H., & Paterson, R. S. (1984). Increased corrosion of stainless steel implants in infected plated fractures. Archives of Orthopaedic and Traumatic Surgery, 102(3), 198–200. https://doi.org/10.1007/bf00575233
  21. Corsini, E. (2000). Epidermal cytokines in experimental contact dermatitis. Toxicology, 142(3), 203–212. https://doi.org/10.1016/s0300-483x(99)00145-6
  22. Sato, Y., Katsumura, Y., Ichikawa, H., Kobayashi, T., Kozuka, T., Morikawa, F., & Ohta, S. (1981). A modified technique of guinea pig testing to identify delayed hypersensitivity allergens. Contact Dermatitis, 7(5), 225–237. https://doi.org/10.1111/j.1600-0536.1981.tb04058.x
  23. Experimental studies on metal dermatitis in guinea pigs
  24. Anderson, C., Sundberg, K., & Groth, O. (1986). Animal model for assessment of skin irritancy. Contact Dermatitis, 15(3), 143–151. https://doi.org/10.1111/j.1600-0536.1986.tb01315.x
  25. Askenase, P. W. (1973). CUTANEOUS BASOPHIL HYPERSENSITIVITY IN CONTACT-SENSITIZED GUINEA PIGS. The Journal of Experimental Medicine, 138(5), 1144–1155. https://doi.org/10.1084/jem.138.5.1144

1–25 of 30

Citations

  1. C, P. R., Babu N B, K., Balaji, N. S., Saikiran, A., & Kannan A, R. (2025). Effect of nutrient-based alloying elements on biodegradable magnesium alloys: Evolution, challenges, and strategies for orthopaedic applications. Biomedical Engineering Advances, 9, 100161. https://doi.org/10.1016/j.bea.2025.100161
  2. https://doi.org/10.1360/sst-2024-0234
  3. https://doi.org/10.3390/ijms25116242
  4. Hashemi, M., Alizadeh, R., & Langdon, T. G. (2023). Recent advances using equal-channel angular pressing to improve the properties of biodegradable Mg‒Zn alloys. Journal of Magnesium and Alloys, 11(7), 2260–2284. https://doi.org/10.1016/j.jma.2023.07.009
  5. Jana, A., Balla, V. K., & Das, M. (2023). In-vitro corrosion and biocompatibility properties of heat treated Mg-4Y-2.25Nd-0.5Zr alloy. Materials Chemistry and Physics, 304, 127873. https://doi.org/10.1016/j.matchemphys.2023.127873
  6. Kasaeian-Naeini, M., Sedighi, M., & Hashemi, R. (2022). Severe plastic deformation (SPD) of biodegradable magnesium alloys and composites: A review of developments and prospects. Journal of Magnesium and Alloys, 10(4), 938–955. https://doi.org/10.1016/j.jma.2021.11.006
  7. Aljohani, T. A., Aljadaan, S., Bin Rubayan, M. T., & Khoshnaw, F. (2021). Impact of processing parameters in plasma electrolytic oxidation on corrosion resistance of magnesium alloy type AZ91. Engineering Reports, 4(2). https://doi.org/10.1002/eng2.12459
  8. Jana, A., Das, M., & Balla, V. K. (2021). In vitro and in vivo degradation assessment and preventive measures of biodegradable Mg alloys for biomedical applications. Journal of Biomedical Materials Research Part A, 110(2), 462–487. https://doi.org/10.1002/jbm.a.37297
  9. Chon, J. W., Xin, Y., Lee, S. M., Kim, Y. J., Jeon, I. S., Jho, J. Y., & Chung, D. J. (2021). In vivo Evaluation of PEEK Copolymer Composites for Prosthetic Spine. Macromolecular Research, 29(3), 244–251. https://doi.org/10.1007/s13233-021-9027-2
  10. SathishKumar, G., Parameswaran, P., Vijayan, V., & Yokeswaran, R. (2021). Effects of Ca, Cu concentration on degradation behavior of Zn alloys in Hank’s solution. Metal Powder Report, 76(1), 40–42. https://doi.org/10.1016/j.mprp.2019.12.005
  11. Lutiyatmi, Sutiyoko, & Afandi, R. (2021). Optimum Load in Vickers Microhardness Testing of Treated Magnesium Alloy by Thermal Oxidation. IOP Conference Series: Materials Science and Engineering, 1082(1), 012002. https://doi.org/10.1088/1757-899x/1082/1/012002
  12. Mena-Morcillo, E., & Veleva, L. (2020). Degradation of AZ31 and AZ91 magnesium alloys in different physiological media: Effect of surface layer stability on electrochemical behaviour. Journal of Magnesium and Alloys, 8(3), 667–675. https://doi.org/10.1016/j.jma.2020.02.014
  13. Lee, J. H., Baek, S. M., Lee, G., Kim, S.-. jong ., Kim, H. S., & Hahn, S. K. (2020). Biocompatible Magnesium Implant Double-Coated with Dexamethasone-Loaded Black Phosphorus and Poly(lactide-co-glycolide). ACS Applied Bio Materials, 3(12), 8879–8889. https://doi.org/10.1021/acsabm.0c01179
  14. Torroni, A., Witek, L., Fahliogullari, H. P., Bortoli, J. P., Ibrahim, A., Hacquebord, J., Gupta, N., & Coelho, P. (2020). WE43 and WE43-T5 Mg alloys screws tested in-vitro cellular adhesion and differentiation assay and in-vivo histomorphologic analysis in an ovine model. Journal of Biomaterials Applications, 35(8), 901–911. https://doi.org/10.1177/0885328220956788
  15. https://doi.org/10.3390/ma13183914
  16. Song, Y. J., Chon, J. W., Yoo, H., Kim, J. H., & Chung, D. J. (2019). Cytotoxicity and In Vivo Biosafety Studies of the Poly(alkylphenol) Derivatives as Vulcanizing Agents. Macromolecular Research, 27(11), 1081–1088. https://doi.org/10.1007/s13233-019-7150-0
  17. Oshibe, N., Marukawa, E., Yoda, T., & Harada, H. (2019). Degradation and interaction with bone of magnesium alloy WE43 implants: A long-term follow-up in vivo rat tibia study. Journal of Biomaterials Applications, 33(9), 1157–1167. https://doi.org/10.1177/0885328218822050
  18. https://doi.org/10.4012/dmj.2017-324
  19. Bircher, A. J. (2018). Metal Allergy: Other Metals. In Metal Allergy (pp. 467–479). Springer International Publishing. https://doi.org/10.1007/978-3-319-58503-1_35
  20. Torroni, A., Xiang, C., Witek, L., Rodriguez, E. D., Flores, R. L., Gupta, N., & Coelho, P. G. (2018). Histo-morphologic characteristics of intra-osseous implants of WE43 Mg alloys with and without heat treatment in an in vivo cranial bone sheep model. Journal of Cranio-Maxillofacial Surgery, 46(3), 473–478. https://doi.org/10.1016/j.jcms.2017.12.028
  21. Mena-Morcillo, E., Veleva, L. P., & Wipf, D. O. (2018). Multi-Scale Monitoring the First Stages of Electrochemical Behavior of AZ31B Magnesium Alloy in Simulated Body Fluid. Journal of The Electrochemical Society, 165(11), C749–C755. https://doi.org/10.1149/2.0291811jes
  22. https://doi.org/10.3390/met8110933
  23. Zhao, S., McNamara, C. T., Bowen, P. K., Verhun, N., Braykovich, J. P., Goldman, J., & Drelich, J. W. (2017). Structural Characteristics and In Vitro Biodegradation of a Novel Zn-Li Alloy Prepared by Induction Melting and Hot Rolling. Metallurgical and Materials Transactions A, 48(3), 1204–1215. https://doi.org/10.1007/s11661-016-3901-0
  24. Cui, L., Sun, L., Zeng, R., Zheng, Y., & Li, S. (2017). In vitro degradation and biocompatibility of Mg-Li-Ca alloys—the influence of Li content. Science China Materials, 61(4), 607–618. https://doi.org/10.1007/s40843-017-9071-y
  25. Radha, R., & Sreekanth, D. (2017). Insight of magnesium alloys and composites for orthopedic implant applications – a review. Journal of Magnesium and Alloys, 5(3), 286–312. https://doi.org/10.1016/j.jma.2017.08.003

1–25 of 66